Material and forging spec
Verify valuesMATERIAL: [4340 STEEL]. FORGE PER [SAE AMS-F-7190 / CUSTOMER SPEC].MATERIAL: [ACERO 4340]. FORJAR SEGÚN [SAE AMS-F-7190 / ESPECIFICACIÓN DEL CLIENTE].Home › Drawing notes › Forging and sand / investment casting
Free drawing notes library
14 copy-ready notes for forging and sand / investment casting, in English and Spanish. Copy a note, replace the [bracketed] example values, and check the "Watch for" line before you release the drawing.
Values in [brackets] are examples; replace them with your own. Notes marked Verify values rely on common practice; confirm them with your supplier or design engineer. These notes are examples, not an engineering approval of your drawing.
FRG-01 Material and forging specFRG-02 Forging tolerancesFRG-03 Parting line, mismatch and flashFRG-04 Scale and surfaceFRG-05 Grain flowFRG-06 Heat treatmentFRG-07 Magnetic particle inspectionFRG-08 Serialization and markingCST-01 AlloyCST-02 Casting tolerancesCST-03 Radiographic qualityCST-04 Weld repairCST-05 Datum targetsCST-06 Surface roughness as cast
MATERIAL: [4340 STEEL]. FORGE PER [SAE AMS-F-7190 / CUSTOMER SPEC].MATERIAL: [ACERO 4340]. FORJAR SEGÚN [SAE AMS-F-7190 / ESPECIFICACIÓN DEL CLIENTE].UNTOLERANCED FORGED DIMENSIONS PER [FORGING INDUSTRY ASSOCIATION TOLERANCES FOR IMPRESSION DIE FORGINGS], [COMMERCIAL] GRADE.DIMENSIONES FORJADAS SIN TOLERANCIA SEGÚN [TOLERANCIAS DE LA FORGING INDUSTRY ASSOCIATION PARA FORJA EN MATRIZ], GRADO [COMERCIAL].PARTING LINE AS SHOWN. DIE MISMATCH [.030] MAX. FLASH EXTENSION AFTER TRIM [.030] MAX. DIE CLOSURE +[.060]/-[.020].LÍNEA DE PARTICIÓN COMO SE MUESTRA. DESALINEACIÓN DE MATRIZ [.030] MÁX. REBABA DESPUÉS DEL RECORTE [.030] MÁX. CIERRE DE MATRIZ +[.060]/-[.020].REMOVE SCALE BY [SHOT BLAST]. SURFACE DEFECTS (LAPS, SEAMS) DEEPER THAN [.015] NOT PERMITTED.RETIRAR LA CASCARILLA CON [GRANALLADO]. NO SE PERMITEN DEFECTOS SUPERFICIALES (TRASLAPES, COSTURAS) MAYORES A [.015] DE PROFUNDIDAD.GRAIN FLOW SAMPLE AT PLANE [△27] REQUIRED ON FIRST ARTICLE.SE REQUIERE MUESTRA DE FLUJO DE GRANO EN EL PLANO [△27] EN EL PRIMER ARTÍCULO.HEAT TREAT PARTS PER AMS 2759/[1] TO [BHN 270–327]. (raw stock: AMS-H-6875)TRATAMIENTO TÉRMICO DE PIEZAS SEGÚN AMS 2759/[1] A [270–327 BHN].MAGNETIC PARTICLE INSPECT PER ASTM E1444. ACCEPTANCE PER [___].INSPECCIÓN POR PARTÍCULAS MAGNÉTICAS SEGÚN ASTM E1444. ACEPTACIÓN SEGÚN [___].SERIALIZE. MARK PART NUMBER AND SERIAL NUMBER PER MIL-STD-130, [ENGRAVED], AT [△28].SERIALIZAR. MARCAR NÚMERO DE PARTE Y NÚMERO DE SERIE SEGÚN MIL-STD-130, [GRABADO], EN [△28].[A356.0-T6] PER ASTM B26. Gray iron: ASTM A48 CLASS [30]. Ductile iron: ASTM A536 [65-45-12]. Carbon steel: ASTM A27 GRADE [70-36].ALUMINIO [A356.0-T6] SEGÚN ASTM B26. (igual para los demás)GENERAL CASTING TOLERANCES: ISO 8062-3, DCTG [10]. (investment: DCTG [6])TOLERANCIAS GENERALES DE FUNDICIÓN: ISO 8062-3, DCTG [10].RADIOGRAPH ZONES MARKED [△29] PER ASTM E1742. ACCEPTANCE PER [ASTM E155 (AL) / E446 (STEEL)], SEVERITY LEVEL [2].RADIOGRAFIAR LAS ZONAS MARCADAS [△29] SEGÚN ASTM E1742. ACEPTACIÓN SEGÚN [ASTM E155 (AL) / E446 (ACERO)], NIVEL [2].WELD REPAIR [NOT PERMITTED / PERMITTED WITH WRITTEN APPROVAL, REPAIR MAP REQUIRED].REPARACIÓN CON SOLDADURA [NO PERMITIDA / PERMITIDA CON APROBACIÓN ESCRITA, CON MAPA DE REPARACIONES].AS-CAST SURFACES [250] µin Ra MAX.SUPERFICIES DE FUNDICIÓN [250] µin Ra MÁX.Fred checks your PDF drawings against ASME Y14.5 and sends a findings report: every correction located by sheet and zone, with what to change and why. From $29 a sheet. NDA first.